Corrugation
The DURVINIL ® sheet, perforated and unperforated, is hotbent by means of equipment which prevents the stretching and the internal stress of the material. The corrugation pitch can change according to the corrugation height.
In the following table are shown the corrugation pitches in relation with the corrugation heights. The corrugation heights, or overall thickness, includes the sheet thickness.
| Pitch mm. | Corrugation mm. | |
| Da | a | |
| 4,65 | 0,8 | 3,3 |
| 5,40 | 3,4 | 3,6 |
| 6,50 | 3,7 | 3,9 |
| 10,00 | 4,5 | 5,0 |